COMMISSION DELEGATED REGULATION (EU) 2016/364
of 1 July 2015
on the classification of the reaction to fire performance of construction products pursuant to Regulation (EU) No 305/2011 of the European Parliament and of the Council
(Text with EEA relevance)
Article 1
Article 2
Article 3
ANNEX
Classes of reaction to fire performance
| 
                   Class  | 
               
                   Test method(s)  | 
               
                   Classification criteria  | 
               
                   Additional classification  | 
            
| 
                   A1  | 
               
                   EN ISO 1182(2); and  | 
               
                   ΔΤ ≤ 30 °C; and Δm ≤ 50 %; and tf = 0 (i.e. no sustained flaming)  | 
               
                   
  | 
            
| 
                   EN ISO 1716  | 
               
                   PCS ≤ 2,0 MJkg– 1 (2); and PCS ≤ 2,0 MJkg– 1 (3) (1); and PCS ≤ 1,4 MJm– 2 (4); and PCS ≤ 2,0 MJkg– 1 (5)  | 
               
                   
  | 
            |
| 
                   A2  | 
               
                   EN ISO 1182(2); or  | 
               
                   ΔΤ ≤ 50 °C; and Δm ≤ 50 %; and tf ≤ 20 s  | 
               
                   
  | 
            
| 
                   EN ISO 1716; and  | 
               
                   PCS ≤ 3,0 MJkg– 1 (2); and PCS ≤ 4,0 MJm– 2 (3); and PCS ≤ 4,0 MJm– 2 (4); and PCS ≤ 3,0 MJkg– 1 (5)  | 
               
                   
  | 
            |
| 
                   EN 13823 (SBI)  | 
               
                   FIGRA ≤ 120 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 7,5 MJ  | 
               
                   Smoke production(6); and Flaming droplets/particles(7)  | 
            |
| 
                   B  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 120 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 7,5 MJ  | 
               
                   Smoke production(6); and Flaming droplets/particles(7)  | 
            
| 
                   EN ISO 11925-2(9): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   C  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 250 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 15 MJ  | 
               
                   Smoke production(6); and Flaming droplets/particles(7)  | 
            
| 
                   EN ISO 11925-2(9): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   D  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 750 Ws– 1  | 
               
                   Smoke production(6); and Flaming droplets/particles(7)  | 
            
| 
                   EN ISO 11925-2(9): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   E  | 
               
                   EN ISO 11925-2(9): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
               
                   Flaming droplets/particles(8)  | 
            
| 
                   F  | 
               
                   EN ISO 11925-2(9): Exposure = 15 s  | 
               
                   Fs > 150 mm within 20 s  | 
               
                   
  | 
            
| 
                   Class  | 
               
                   Test method(s)  | 
               
                   Classification criteria  | 
               
                   Additional classification  | 
            
| 
                   A1FL  | 
               
                   EN ISO 1182(10); and  | 
               
                   ΔΤ ≤ 30 °C; and Δm ≤ 50 %; and tf = 0 (i.e. no sustained flaming)  | 
               
                   
  | 
            
| 
                   EN ISO 1716  | 
               
                   PCS ≤ 2,0 MJkg– 1 (10); and PCS ≤ 2,0 MJkg– 1 (11); and PCS ≤ 1,4 MJm– 2 (12); and PCS ≤ 2,0 MJkg– 1 (13)  | 
            ||
| 
                   A2FL  | 
               
                   EN ISO 1182(10); or  | 
               
                   ΔΤ ≤ 50 °C; and Δm ≤ 50 %; and tf ≤ 20 s  | 
               
                   
  | 
            
| 
                   EN ISO 1716; and  | 
               
                   PCS ≤ 3,0 MJkg– 1 (10); and PCS ≤ 4,0 MJm– 2 (11); and PCS ≤ 4,0 MJm– 2 (12); and PCS ≤ 3,0 MJkg– 1 (13)  | 
            ||
| 
                   EN ISO 9239-1(14)  | 
               
                   Critical flux(15) ≥ 8,0 kWm– 2  | 
               
                   Smoke production(16)  | 
            |
| 
                   BFL  | 
               
                   EN ISO 9239-1(14) and  | 
               
                   Critical flux(15) ≥ 8,0 kWm– 2  | 
               
                   Smoke production(16)  | 
            
| 
                   EN ISO 11925-2(17): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
            ||
| 
                   CFL  | 
               
                   EN ISO 9239-1(14) and  | 
               
                   Critical flux(15) ≥ 4,5 kWm– 2  | 
               
                   Smoke production(16)  | 
            
| 
                   EN ISO 11925-2(17): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
            ||
| 
                   DFL  | 
               
                   EN ISO 9239-1(14) and  | 
               
                   Critical flux(15) ≥ 3,0 kWm– 2  | 
               
                   Smoke production(16)  | 
            
| 
                   EN ISO 11925-2(17): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
            ||
| 
                   EFL  | 
               
                   EN ISO 11925-2(17): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
               
                   
  | 
            
| 
                   FFL  | 
               
                   EN ISO 11925-2(17): Exposure = 15 s  | 
               
                   Fs > 150 mm within 20 s  | 
               
                   
  | 
            
| 
                   Class  | 
               
                   Test method(s)  | 
               
                   Classification criteria  | 
               
                   Additional classification  | 
            
| 
                   A1L  | 
               
                   EN ISO 1182(18); and  | 
               
                   ΔT ≤ 30 °C; and Δm ≤ 50 %; and tf = 0 (i.e. no sustained flaming)  | 
               
                   
  | 
            
| 
                   EN ISO 1716  | 
               
                   PCS ≤ 2,0 MJkg– 1 (18); and PCS ≤ 2,0 MJkg– 1 (19); and PCS ≤ 1,4 MJm– 2 (20); and PCS ≤ 2,0 MJkg– 1 (21)  | 
            ||
| 
                   A2L  | 
               
                   EN ISO 1182(18); or  | 
               
                   ΔT ≤ 50 °C; and Δm ≤ 50 %; and tf ≤ 20 s  | 
               
                   
  | 
            
| 
                   EN ISO 1716; and  | 
               
                   PCS ≤ 3,0 MJkg– 1 (18); and PCS ≤ 4,0 MJm– 2 (19); and PCS ≤ 4,0 MJm– 2 (20); and PCS ≤ 3,0 MJkg– 1 (21)  | 
            ||
| 
                   EN 13823 (SBI)  | 
               
                   FIGRA ≤ 270 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 7,5 MJ  | 
               
                   Smoke production(22); and Flaming droplets/particles(23)  | 
            |
| 
                   BL  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 270 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 7,5 MJ  | 
               
                   Smoke production(22); and Flaming droplets/particles(23)  | 
            
| 
                   EN ISO 11925-2(25): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   CL  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 460 Ws– 1; and LFS < edge of specimen; and THR600s ≤ 15 MJ  | 
               
                   Smoke production(22); and Flaming droplets/particles(23)  | 
            
| 
                   EN ISO 11925-2(25): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   DL  | 
               
                   EN 13823 (SBI); and  | 
               
                   FIGRA ≤ 2 100 Ws– 1 THR600s ≤ 100 MJ  | 
               
                   Smoke production(22); and Flaming droplets/particles(23)  | 
            
| 
                   EN ISO 11925-2(25): Exposure = 30 s  | 
               
                   Fs ≤ 150 mm within 60 s  | 
            ||
| 
                   EL  | 
               
                   EN ISO 11925-2(25): Exposure = 15 s  | 
               
                   Fs ≤ 150 mm within 20 s  | 
               
                   Flaming droplets/particles(24)  | 
            
| 
                   FL  | 
               
                   EN ISO 11925-2(25): Exposure = 15 s  | 
               
                   Fs > 150mm within 20 s  | 
               
                   
  | 
            
| 
                   Class  | 
               
                   Test method(s)  | 
               
                   Classification criteria  | 
               
                   Additional classification  | 
            
| 
                   Aca  | 
               
                   EN ISO 1716  | 
               
                   PCS ≤ 2,0 MJ/kg(26)  | 
               
                   
  | 
            
| 
                   B1ca  | 
               
                   EN 50399 (30 kW flame source) and  | 
               
                   FS ≤ 1,75 m and THR1200s ≤ 10 MJ and Peak HRR ≤ 20 kW and FIGRA ≤ 120 Ws– 1  | 
               
                   Smoke production(27) (30) and Flaming droplets/particles(28) and Acidity (pH and conductivity)(29)  | 
            
| 
                   EN 60332-1-2  | 
               
                   H ≤ 425 mm  | 
            ||
| 
                   B2ca  | 
               
                   EN 50399 (20,5 kW flame source) and  | 
               
                   FS ≤ 1,5 m; and THR1200s ≤ 15 MJ; and Peak HRR ≤ 30 kW; and FIGRA ≤ 150 Ws– 1  | 
               
                   Smoke production(27) (31) and Flaming droplets/particles(28) and Acidity (pH and conductivity)(29)  | 
            
| 
                   EN 60332-1-2  | 
               
                   H ≤ 425 mm  | 
            ||
| 
                   Cca  | 
               
                   EN 50399 (20,5 kW flame source) and  | 
               
                   FS ≤ 2,0 m; and THR1200s ≤ 30 MJ; and Peak HRR ≤ 60 kW; and FIGRA ≤ 300 Ws– 1  | 
               
                   Smoke production(27) (31) and Flaming droplets/particles(28) and Acidity (pH and conductivity)(29)  | 
            
| 
                   EN 60332-1-2  | 
               
                   H ≤ 425 mm  | 
            ||
| 
                   Dca  | 
               
                   EN 50399 (20,5 kW flame source) and  | 
               
                   THR1200s ≤ 70 MJ; and Peak HRR ≤ 400 kW; and FIGRA ≤ 1 300 Ws– 1  | 
               
                   Smoke production(27) (31) and Flaming droplets/particles(28) and Acidity (pH and conductivity)(29)  | 
            
| 
                   EN 60332-1-2  | 
               
                   H ≤ 425 mm  | 
            ||
| 
                   Eca  | 
               
                   EN 60332-1-2  | 
               
                   H ≤ 425 mm  | 
               
                   
  | 
            
| 
                   Fca  | 
               
                   EN 60332-1-2  | 
               
                   H > 425 mm  | 
               
                   
  |